MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Composiflex FlexPLY™ High Performance Composite Spring, Crossply 1:1
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: A variety of carbon/epoxy, E-glass epoxy, and high-temperature glass/epoxy springs and available for industrial equipment uses. Some examples of these types of machinery include conveyors, oscillating sanders, vibratory rollers, vibratory feeders, and more.

Crossply - Fibers alternate 0° and 90° at specified intervals, typically 1:1. Example 0,90,0,90,0,90,0.
Available thickness per ply: 0.005 in. and 0.010 in.

Mechanical property data measured on 0.15 in thick samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 6767
Tensile Strength  434 MPa
@Temperature 71.1 °C
62900 psi
@Temperature 160 °F
ASTM D3039
 484 MPa
@Temperature 22.8 °C
70200 psi
@Temperature 73.0 °F
ASTM D3039
Tensile Modulus  30.3 GPa
@Temperature 71.1 °C
4390 ksi
@Temperature 160 °F
Chord Modulus from 0.1 to 0.3%, P; ASTM D3039
 32.4 GPa
@Temperature 22.8 °C
4700 ksi
@Temperature 73.0 °F
Chord Modulus from 0.1 to 0.3%, P; ASTM D3039
Flexural Strength  583 MPa
@Temperature 71.1 °C
84600 psi
@Temperature 160 °F
ASTM D790
 636 MPa
@Temperature 22.8 °C
92300 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus  22.1 GPa
@Temperature 71.1 °C
3210 ksi
@Temperature 160 °F
ASTM D790
 23.9 GPa
@Temperature 22.8 °C
3470 ksi
@Temperature 73.0 °F
ASTM D790
Compressive Strength  349 MPa
@Temperature 71.1 °C
50600 psi
@Temperature 160 °F
ASTM D3410
 466 MPa
@Temperature 22.8 °C
67600 psi
@Temperature 73.0 °F
ASTM D3410
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.82
@Frequency 1e+6 Hz
4.82
@Frequency 1e+6 Hz
50% RH; ASTM D150
 4.98
@Frequency 100000 Hz
4.98
@Frequency 100000 Hz
50% RH; ASTM D150
 5.17
@Frequency 1000 Hz
5.17
@Frequency 1000 Hz
50% RH; ASTM D150
 5.25
@Frequency 60 Hz
5.25
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 16.9 kV/mm428 kV/in50% RH; ASTM D149
Dissipation Factor  0.0070
@Frequency 60 Hz
0.0070
@Frequency 60 Hz
50% RH; ASTM D150
 0.0080
@Frequency 1000 Hz
0.0080
@Frequency 1000 Hz
50% RH; ASTM D150
 0.018
@Frequency 100000 Hz
0.018
@Frequency 100000 Hz
50% RH; ASTM D150
 0.038
@Frequency 1e+6 Hz
0.038
@Frequency 1e+6 Hz
50% RH; ASTM D150
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 129 °C265 °FDMA, E'

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOMPOS92 / 282296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.