MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Gravi-Tech™ GRV-TE1-060-W-NAT Styrene Isoprene Styrene Block Copolymer (SIS)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 5.99 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.017 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
 
Processing PropertiesOriginal ValueComments
Melt Temperature 163 - 204 °C
Mold Temperature 15.6 - 37.8 °C
Drying Temperature 76.7 °C
 
Descriptive Properties
AppearanceNatural Color
FeaturesHigh Specific Gravity
 Non-Toxic
FormsPellets
Generic MaterialSIS
Generic NameStyrene Isoprene Styrene Block Copolymer (SIS)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesIndustrial Applications
 Medical/Healthcare Applications
 Projectiles
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray SEPTON® S2063 Thermoplastic Rubber
Kuraray SEPTON® S4033 Thermoplastic Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
Ecomass® Ecomass® 5033ZC87 SS Powder filled Styrene Isoprene Styrene (SIS)

PH0POL1245 / 145814

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.