MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: AAROPRENE® ATPR 2000 Series Elastomeric Compound

Features: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Melt Flow 15 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40ASTM D2240
Tensile Strength at Break 900 psiASTM D412
Elongation at Break 800 %ASTM D412
Tensile Modulus 180 psiASTM D412
Taber Abrasion, mg/1000 Cycles 290ASTM D1044
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °F
Nozzle Temperature 455 °F
Injection Pressure 500 - 700 psi
Back Pressure 50.0 psi
Cycle Time - Injection 1.0 sec
Screw Speed 40 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRONAA924 / 135255

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.