MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding product range. It is processable at low temperatures and offers a specially designed, flexible material suitable for moldings.

Performance Features:

  • High transparency
  • Soft type
  • Good melt flow
  • Phthalate free
  • High elasticity
  • Easy coloring

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccInjection molded; ASTM D792
Linear Mold Shrinkage 0.0090 in/inInjection molded; ASTM D955
Melt Index of Compound 30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68Injection molded parts; ASTM D2240
Hardness, Shore D 20Injection molded parts; ASTM D2240
Tensile Strength at Break 45.0 MPa0.025" extruded film,; DIN 53504
Elongation at Break 770 %0.025" extruded film; DIN 53504
100% Modulus 0.00340 GPa
@Strain 100 %
0.025" extruded film; DIN 53504
300% Modulus 0.00700 GPa
@Strain 300 %
0.025" extruded film; DIN 53504
Tear Strength 257 pli0.025" extruded film; DIN 53515
Abrasion 30mm3, Injection molded; DIN 53516
Compression Set 34 %
@Temperature 22.8 °C,
Time 252000 sec
Injection molded; ASTM D395
 48 %
@Temperature 70.0 °C,
Time 86400 sec
Injection molded; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 120 - 165 °C0.025" extruded film,
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °C
Middle Barrel Temperature 180 °C
Adapter Temperature 180 °C
Die Temperature 170 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester

PHUQ088 / 159461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.