MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NAECO® NAECOMET® D50F Silver Nickel Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices where auxiliary contacts are used. This type of material has good resistance to mechanical wear under high contact forces, and maintains a stable surface resistance.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.3074 g/cc0.33625 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 4040annealed
 8989cold worked
Tensile Strength, Ultimate 186 MPa27000 psiannealed
 345 MPa50000 psicold worked
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000220 ohm-cm0.00000220 ohm-cm80 % IACS
 
Component Elements PropertiesMetricEnglishComments
Nickel, Ni 15 %15 %
Silver, Ag 85 %85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® ELKONIUM 18 silver, copper, cadmium alloy
CMW® D510F Silver Nickel Contact Material ASTM B693
CMW® D50F Silver Nickel Alloy
CMW® D505F Silver Nickel Contact Material
CMW® D50 Silver Nickel Contact Material ASTM B693

NCMV877 / 192361

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.