MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Videolar-Innova 825 High Impact Polystyrene (HIPS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes:
  • Injection molding grade
  • Medium melt flow and high gloss
  • Good balance between rigidity and impact
Features:
  • Excellent mechanical strength
  • Excellent temperature resistance
  • high impact
Applications:
  • Toys, appliance parts, construction, packaging, and structural foam

Information provided by Dax Resinas

Key Words: FDA 21 CFR 177.1640
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.650 g/ccISO 060
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
Melt Flow 6.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23.0 MPaASTM D638
Elongation at Yield 50 %ASTM D638
Tensile Modulus 2.14 GPaASTM D638
Flexural Strength 44.0 MPaASTM D790
Flexural Modulus 2280 MPaASTM D790
Izod Impact, Notched 107 J/mASTM D256
Falling Dart Impact 14.0 JASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C@ 264 psi; ASTM D648
Vicat Softening Point 96.0 °CASTM D1525
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Videolar-Innova 825 E High Impact Polystyrene (HIPS)
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene
Chevron Phillips EB6400 HIPS - High Impact Polystyrene
Americas Styrenics EB6755 High Impact Polystyrene

PDAX000 / 29425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.