MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H65-175MP Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® H65-175MP is a single component, alumina-filled epoxy for military hybrid die and component attach. It can also be used for semiconductor and high temperature ceramic and vacuum packaging.

Advantages & Application Notes:

  • Viscosity is suitable for automatic syringe dispensers, although it can be applied by screen printing or manual hand Operations.
  • Performs exceptionally well as a die-attach for small chips such as GaAs, LEDs and diodes, as well as SMDs.
  • Capable of resisting 260°C green reflow process, low outgassing in hermetic lid-seal processes near 300°C, and organic burn-in up to 150°C/1000 hours storage.
  • Certified to MIL-STD 883/Test Method 5011 –yields low levels of water extractable monovalent ions such as Chlorides.
  • Capable of JEDEC Level II die-attach packaging on die-paddles and lead-frames.
  • Widely used epoxy; popular choice for non-silver-filled die-attach epoxies; opto-packaging, hybrids, and many types of substrates including kovar, ceramic and BT.
  • Available in many different viscosity ranges
  • Can be used as non conductive staking epoxy, in conjunction with EPO-TEK® H35-175MP for attaching SMDs to the hybrid circuit.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.68 g/cc
Particle Size <= 20 µm
Viscosity 80000 - 120000 cP
@Temperature 23.0 °C
2.5 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) <= 50 ppm
Ionic Impurities - K (Potassium) <= 50 ppm
Ionic Impurities - Cl (Chloride) <= 200 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 95
Tensile Modulus 816000 psiStorage
Shear Strength >= 2000 psiLap
 >= 6800 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.20e+14 ohm-cm
Dielectric Constant 5.3
@Frequency 1000 Hz
Dissipation Factor 0.011
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°CBelow Tg
 136 µm/m-°CAbove Tg
Thermal Conductivity 0.794 W/m-K
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 397 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 180 °C
Minimum Bond Line
Pot Life 40320 min
Shelf Life 12.0 Month
@Temperature -40.0 °C
 
Descriptive Properties
ColorWhite
ConsistencySmooth paste
Ionic Impurities NH438 ppm
Number of ComponentsSingle
Thixotropic Index1.87
Weight Loss0.1%200°C
 0.16%250°C
 0.3%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PPT FP95 Fully Sintered Ferrite Powder
Epoxy Technology EPO-TEK® H67MP-T Thermally Conductive, Electrically Insulating Epoxy
Copper, Cu; Annealed
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive

PPOXYT067 / 141106

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.