MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 3139D Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3100 series are engineered materials designed primarily general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. Sarlink 3139D, available in NAT and BLK, is a hard hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Fatigue Resistant; Good Adhesion; Good Moldability; Good Processability; Good Surface Finish; Medium Heat Resistance; Low Density; High Hardness; Low Specific Gravity; Resilient; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Grommets; Industrial Applications; Plugs; Profiles; Weatherstripping

RoHS Compliance: RoHS Compliant

Automotive Specifications: GM QK 000060 Type A Color: Black; GM QK 3532 Type 2 Color: Natural, Black; PSA Peugeot-Citroen B62 0300 version G Color: Black; RENAULT F.E.M. 03 20 007 Color: Black; TOYOTAL TSM 5529G Color: Black; VAG VW501 23 Color: Black; VOLKSWAGEN TL 1010 Color: Black; VOLKSWAGEN VW 50180 Color: Black

Agency Ratings: UL 94

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Viscosity 310 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
@Time 5.00 sec
Extruded; ISO 868
 41
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 2520 psiFlow; ISO 37
 2680 psiAcross Flow; ISO 37
 2490 psi
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
 2550 psi
@Treatment Temp. 135 °C,
Time 360000 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 1290 psi
@Strain 100 %
Across Flow; ISO 37
 1930 psi
@Strain 100 %
Flow; ISO 37
 1410 psi
@Strain 100 %,
Treatment Temp. 135 °C
Across Flow, Change in Air, 1000 hr; ISO 188
 1430 psi
@Strain 100 %,
Treatment Temp. 150 °C
Across Flow, Change in Air, 168 hr; ISO 188
Elongation at Break 400 %Flow; ISO 37
 700 %Across Flow; ISO 37
 1320 %
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
 1330 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air; ISO 188
Tear Strength 580 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 53 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 67 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 85 %
@Temperature 90.0 °C,
Time 252000 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 122 °FUL 746
UL RTI, Mechanical with Impact 122 °FUL 746
UL RTI, Mechanical without Impact 122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Processing Temperature 365 - 428 °FInjection, Melt
Rear Barrel Temperature 356 - 419 °FInjection
Middle Barrel Temperature 356 - 419 °FInjection
Front Barrel Temperature 356 - 419 °FInjection
Nozzle Temperature 369 - 420 °FInjection
Zone 1 356 - 392 °FExtrusion
Zone 2 356 - 401 °FExtrusion
Zone 3 369 - 410 °FExtrusion
Zone 4 369 - 410 °FExtrusion
Die Temperature 383 - 419 °FExtrusion
Melt Temperature 383 - 419 °FExtrusion
Mold Temperature 50.0 - 131 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 14.5 - 145 psiInjection
Screw Speed 100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo INSPIRE™ TF1500 ESU Polypropylene
Trinseo INSPIRE™ TF1302 Thermoplastic Polyolefin

PTEKNQ1138 / 237629

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.