MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation Bisco® L3 Premiere Dynamic Flooring Material
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: BISCO® L3 Premiere silicone foam technology is the next generation in dynamic and floating floor materials from Rogers Corporation developed specifically to meet the most challenging global requirements for flammability, smoke and toxicity.

The L3 Premiere exhibits a low natural frequency and is engineered to isolate vibration enabling a safe and smooth passenger ride over the life-time of mass transit vehicles.

  • Railcar dynamic and floating floor pads
  • Boat and yacht flooring isolation pads

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.304 g/ccASTM D1056
Water Absorption <= 5.0 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 psiASTM D142
Elongation at Break 50 %ASTM D412
Compressive Yield Strength 16.0 psi
@Strain 25 %
ASTM D1056
Compression Set <= 5.0 %
@Temperature 100 °C,
Time 79200 sec
ASTM D1056
 
Descriptive Properties
Mechanical Loss Factor0.2DMA
Stiffness Factor1.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROGA905 / 138345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.