MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AdvanSix Capran® NyLid™ OMBS-100M Nylon 6/EVOH Lidding Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH); Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Capran® NyLid™ OMBS-100M is a mono-axially oriented, co-extruded Nylon 6/EVOH/Nylon 6 clear film with a print/lamination receptive coating having excellent gas barrier through a broad range of relative humidity. The film provides high strength, good chemical resistance, and excellent flavor and aroma barrier for food packaging.

Applications: Capran® NyLid™ OMBS-100 M is suitable for die cutting, readily accepts printing, accepts heal seal coatings and lacquers, offers excellent puncture resistance, is safe for microwave use, and resists tear propagation. It is ideally suited for lamination, and is FDA compliant for indirect food contact.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.145 g/ccASTM D1505
Oxygen Transmission Rate 1.55 cc/m²/day73°F - 65%RH; ASTM D3985
 1.55 cc/m²/day73°F - 0%RH; ASTM D3985
Surface Tension >= 64 dynes/cmcoated side
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 70 %ASTM D882
Film Elongation at Break, TD 375 %ASTM D882
Tear Strength Test 1100graves tear MD, grams/mil; ASTM D1004
 1300graves tear TD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 46000 psiASTM D882
Film Tensile Strength at Break, TD 14000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD -6.50 %
@Temperature 177 °C,
Time 601 sec
ASTM D1204
Shrinkage, TD -1.00 %
@Temperature 177 °C,
Time 601 sec
ASTM D1204
 
Optical PropertiesOriginal ValueComments
Haze <= 6.0 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
DuPont Selar® RB 421 EVOH Barrier Resin
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
Soarus SoarnoL® DT2903 Ethylene Vinyl Alcohol Copolymer
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film

PALC033 / 23795

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.