Product Description: Key Features- 35-mesh powder
- Excellent long term outdoor weatherability (UV8)
- Balance of toughness and rigidity
- Excellent low temperature impact
- Good environmental stress crack resistance, ESCR
- Compounded for uniform additive dispersion
- Standard, custom or special effect colors available
- Excellent opacity available in colors
- Standard, custom and natural colors available
- Stock colors may be available. See Stock color bulletin
- UL component recognition listing (E141240)
- Also available in powder form as HMP-304
Availability: North America Features: Good Stiffness; Good Toughness; Good Weather Resistance; High ESCR (Stress Crack Resist.); High Rigidity; Low Temperature Impact Resistance UL File Number: E141240 Appearance: Colors Available; Natural Color; Opaque Form: Powder Processing Method: Rotational Molding Information provided by Ravago Manufacturing Americas |