MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® RE15022 NC010 Polyethylene Terephthalate (PET)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 40% Glass Reinforced

Material Notes: 36% Glass Reinforced Polyethylene Terephthalate

Rynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D792
Density 1.65 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 205 MPaISO 527-1/-2
Tensile Strength 195 MPaASTM D638
Elongation at Break 2.4 %ISO 527-1/-2
 2.4 %ASTM D638
Tensile Modulus 14000 MPaISO 527-1/-2
Izod Impact, Unnotched (ISO) 1180 kJ/m²ASTM D4812
Izod Impact Resistance 10.5 J/cm²ASTM D256
 11.0 J/cm²ASTM D256
Charpy Impact Unnotched 65.0 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 247 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75-1/-2
 235 °CASTM D648
 
Descriptive Properties
Delivery formPellets
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Rynite® 408 NC010 PET
Celanese Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
DuPont Mobility and Materials Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin

PZDSY5284 / 161111

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.