Lewatit® Regler ZL is a strongly acidic, polymer-based resin in powder from with sulfonic acid groups and is ideally suited as a heterogeneous catalyst for organic reactions. A large surface area and good temperature stability give it a high degree of reactivity. Optimum performance is achieved in anhydrous media Applications: - Oligomerization of isobutene
Information provided by Lanxess. |