MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethane

Applications: Instrument panel substrates, consoles, Cluster housing, interior trim

Injection Speed: Medium-Fast

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Filler Content 20 %Glass Fiber
Water Absorption 0.11 %ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmNOVA
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 98.0 MPaASTM D638
Elongation at Break 1.9 %ASTM D638
Tensile Modulus 7.70 GPaASTM D638
Flexural Yield Strength 160 MPaASTM D790
Flexural Modulus 7.10 GPaASTM D790
Poissons Ratio 0.345ASTM D638
Shear Modulus 2.86 GPaCalculated
Izod Impact, Notched 0.840 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°C
@Temperature 20.0 °C
NOVA
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
@Diameter 3.17 mm
bar; ASTM D648
Vicat Softening Point 123 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 249 - 288 °CProfile Temperature
Melt Temperature 260 - 288 °CAir purge at equilibrium conditions
Mold Temperature 43.0 - 60.0 °CMold surface temperature at equilibrium conditions
Back Pressure 50.0 - 100 psi
Screw Speed 80 - 125 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
G-10 Fiberglass Epoxy Laminate Sheet
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
Overview of materials for Thermoset Polyester Glass Filled BMC

PNOVA217 / 55118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.