MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay APC-2/IM7 PEEK with Carbon Fiber Reinforced Unidirectional Tape
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Cytec Engineered Materials APC-2 composites have a thermoplastic matrix of poly(ether-ether-ketone) commonly referred to as PEEK. The polymer is semi-crystalline with a glass transition temperature of 289°F (143°C). Composites can be used in lightly loaded applications at temperatures up to 500°F (260°C) due to the semi-crystalline nature of the polymer. The composites possess excellent environmental resistance, toughness and fire resistant properties. APC-2 prepreg can be stored at ambient conditions and has an indefinite shelf life. APC02 composites retain good mechanical properties at cryogenic temperatures. The excellent composite properties result from the PEEK matrix, the full wetting and tailored fiber matrix interface achieved in the impregnation process. Laminates and parts can be fabricated from APC-2 using a wide range of processes from autoclave consolidation to rapid stamping techniques. The prepreg may also be filament wound and tape-placed using in-situ consolidation. This wide range of processing techniques may be used because of the thermoplastic nature of the polymer and the full wetting of the fibers in the prepreg.

Features & Benefits:

  • Fully impregnated, unidirectional prepreg
  • Large database
  • Very high toughness and damage tolerance
  • Good resistance to creep and fatigue
  • Very good wear resistance
  • Processed using a wide range of fabrication techniques at 720°F (382°C)
Applications: Typical applications for Cytec Engineered Materials APC-2 include aircraft structure, space components and other structural engineering components

Typical property data for composite laminate with 60 volume % IM7 high strength [> 750 ksi (5170 MPa) intermediate modulus [40 Msi (276 GPa) class] carbon fiber reinforced unidirectional tape. Cytec Engineered Materials product code: APC-2/IM7

Information provided by Cytec, subsequently acquired by Solvay.

Key Words: APC-2-PEEK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccUnreinforced PEEK
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7000 psi
@Temperature 177 °C
90° Orientation
 8700 psi
@Temperature 24.0 °C
90° Orientation
 9200 psi
@Temperature -55.0 °C
90° Orientation
 400000 psi
@Temperature 177 °C
0° Orientation
 410000 psi
@Temperature -55.0 °C
0° Orientation
 420000 psi
@Temperature 24.0 °C
0° Orientation
Elongation at Break 1.4 %
@Temperature 177 °C
0° Orientation
 1.5 %
@Temperature -55.0 °C
0° Orientation
 1.5 %
@Temperature 24.0 °C
0° Orientation
Tensile Modulus 8.30 GPa
@Temperature 177 °C
90° Orientation
 10.0 GPa
@Temperature 24.0 °C
90° Orientation
 11.0 GPa
@Temperature -55.0 °C
90° Orientation
 172 GPa
@Temperature -55.0 °C
0° Orientation
 172 GPa
@Temperature 24.0 °C
0° Orientation
 172 GPa
@Temperature 177 °C
0° Orientation
Flexural Strength 13000 psi
@Temperature 177 °C
90° Orientation
 13000 psi
@Temperature 177 °C
90° Orientation, after water immersion for 14 days at 160°F (71°C)
 15000 psi
@Temperature 24.0 °C
90° Orientation
 16000 psi
@Temperature -55.0 °C
90° Orientation
 260000 psi
@Temperature 177 °C
0° Orientation
 260000 psi
@Temperature 177 °C
0° Orientation, after water immersion for 14 days at 160°F (71°C)
 315000 psi
@Temperature 24.0 °C
0° Orientation
 350000 psi
@Temperature -55.0 °C
0° Orientation
Flexural Modulus 7.60 GPa
@Temperature 177 °C
90° Orientation
 7.60 GPa
@Temperature 177 °C
90° Orientation, after water immersion for 14 days at 160°F (71°C)
 9.70 GPa
@Temperature -55.0 °C
90° Orientation
 9.70 GPa
@Temperature 24.0 °C
90° Orientation
 152 GPa
@Temperature 177 °C
0° Orientation
 152 GPa
@Temperature 177 °C
0° Orientation, after water immersion for 14 days at 160°F (71°C)
 159 GPa
@Temperature -55.0 °C
0° Orientation
 159 GPa
@Temperature 24.0 °C
0° Orientation
Compressive Strength 366 MPaafter 1500 in-lb/in (6.67 J/mm) impact
 1170 MPa
@Temperature 177 °C
0° Orientation
 1170 MPa
@Temperature 177 °C
0° Orientation, after water immersion for 14 days at 160°F (71°C)
 1310 MPa
@Temperature 24.0 °C
0° Orientation
 1510 MPa
@Temperature -55.0 °C
0° Orientation
Compressive Modulus 145000 MPa
@Temperature 177 °C
0° Orientation
 145000 MPa
@Temperature 177 °C
0° Orientation, after water immersion for 14 days at 160°F (71°C)
 152000 MPa
@Temperature -55.0 °C
0° Orientation
 152000 MPa
@Temperature 24.0 °C
0° Orientation
Poissons Ratio 0.26
@Temperature -55.0 °C
0° Orientation
 0.27
@Temperature 24.0 °C
0° Orientation
 0.30
@Temperature 177 °C
0° Orientation
Shear Modulus 2.80 GPa
@Temperature 177 °C
In-plane, after water immersion for 14 days at 160°F (71°C)
 3.60 GPa
@Temperature 177 °C
In-plane
 5.50 GPa
@Temperature 24.0 °C
In-plane
 5.90 GPa
@Temperature -55.0 °C
In-plane
Shear Strength 19000 psi
@Temperature 177 °C
In-plane, after water immersion for 14 days at 160°F (71°C)
 20000 psi
@Temperature 177 °C
In-plane
 26000 psi
@Temperature 24.0 °C
In-plane
 28000 psi
@Temperature -55.0 °C
In-plane
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °Flight load
Glass Transition Temp, Tg 143 °CUnreinforced PEEK

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay APC-2/AS4 PEEK Plus Carbon Fiber Reinforced Unidirectional Tape
Solvay MTM® 49-3 Epoxy Prepreg with 36% T1000 GB-124 Carbon Fiber
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Hexcel® HexTow® IM7 6K Intermediate Modulus Carbon Fiber (6000 Filaments)
Hexcel® HexTow® IM7 Carbon Fiber - Epoxy Composite

PCYTED073_3 / 192719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.