A hexane linear low density polyethylene Typical Applications: - Industrial liners
- Stretch wrap
- Garment and carrier bags
- General purpose packaging
Features: - Good stiffness at thin gauges
- Excellent processing characteristics
- Processing aid: yes
- Slip: zero
- Anti-block: 7500 ppm
Information provided by Southern Polymer |