MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Mxsten CV77519 Polyethylene Plastomer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin exhibit exceptionally low seal initiation temperature with a broad hot tack window combined with good stiffness. Other features of this resin include extreme strength in cold and refrigerated temperature environments, high resistance to tears, and high MVTR. Its applications include: agricultural tubing, blown film, food packaging, and trash bags. This resin grade complies with 21 CFR 177.1520. Extrusion conditions used to produce 1 mil (0.025 mm) film include a 6� die, 2.5� 24:1 L:D barrier screw, 2.4:1 BUR, 100-mil die gap, 15� frostline height, 450� F melt temperature, and 7.5 lb/hr/inch die output. Density results are on Base Resin.

Key Words: Low seal initiation temperature with a broad hot tack window combined with good stiffness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.906 g/ccASTM-D4883
Thickness 1.00 mil
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 62.0 MPaASTM-D882
Film Tensile Strength at Yield, TD 8.00 MPaASTM-D882
Film Elongation at Break, MD 600 %ASTM-D822
Film Elongation at Break, TD 1000 %ASTM-D882
Elmendorf Tear Strength MD 600 gASTM-D1992
Elmendorf Tear Strength TD 650 gASTM-D1992
Dart Drop Test >= 2000 gASTM-D1709A
Film Tensile Strength at Break, MD 62.0 MPaASTM-D882
Film Tensile Strength at Break, TD 45.0 MPaASTM-D882
1% Secant Modulus, MD 18000 psiASTM-D822
1% Secant Modulus, TD 21000 psiASTM-D822
Heat Seal Strength Initiation Temperature 82.0 °CTemperature at which 200 g/in. seal strength is achieved.; Westlake Test
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ASTM-D1003
Gloss 60 %Angle 45°; ASTM-D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Mxsten CV77529 Polyethylene Plastomer
Westlake Mxsten CV77512 Polyethylene Plastomer

PWESF9002 / 106839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.