MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dover Chemical MAYSYN S122 Synthetic Fluid Concentrate Grinding and Medium Duty Machining
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Maysyn S-122 is an oil-rejecting synthetic coolant concentrate formulated for all types of metals and alloys, including cast iron, steels, stainless, and nonferrous materials. This coolant contains no DEA, chlorinated, sulfurized, or phosphorus-containing additives. Maysyn S-122 is also fortified against microorganism attack through the incorporation of a bactericide/fungicide package. Maysyn S-122 is designed to be cutback with water at a ratio of 60/40 (water/product) before providing the coolant to your customers. This final cutback offers excellent corrosion inhibition (no corrosion @ 24 hours at 33:1 dilution), good hard water stability (transparent solution @ 24 hours in 600ppm H20), low foam tendency, and complete oil rejecting properties for clean running machines and parts. This product is to be kept from freezing.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
@Temperature 15.6 °C
60/60°F
Density 8.90 lb/gal
pH 9.45% concentration
 10.2Neat
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 90
 
Descriptive Properties
AppearanceClear Yellow
Total Alkalinity18[meqKOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER143 / 217762

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.