NIKROTHAL 20 is used at operating temperatures up to 1050°C (1920°F). Typical applications for NIKROTHAL 20 are as terminals attached to nickel-chromium heating elements operating at relatively low temperatures and in other applications where the material is exposed to elevated temperature. Information provided by Sandvik |