MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultraform® S 1320 0021 AT POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Ultraform® S 1320 0021 AT is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels, including hot diesel fuel. Typical applications include fuel tank components requiring resistance to hot diesel fuel. Typical applications include fuel tank components requiring resistance to hot diesel fuel.

Availability: North America

Features: Fuel Resistant; Good Flow; Good Heat Resistance; Good Stiffness

Use: Fuel Tanks

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 0.25 %0.25 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.90 %0.90 %ISO 62
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cm0.021 in/inISO 294-4
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 67.0 MPa9720 psiISO 527-2
Elongation at Break 25 %25 %Nominal; ISO 527-2
Elongation at Yield 10 %10 %ISO 527-2
Tensile Modulus 3.00 GPa435 ksiISO 527-1
Izod Impact, Notched (ISO) 5.46 kJ/m²2.60 ft-lb/in²ISO 180
Charpy Impact Unnotched  23.1 J/cm²
@Temperature -30.0 °C
110 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 27.3 J/cm²
@Temperature 22.8 °C
130 ft-lb/in²
@Temperature 73.0 °F
ISO 179
Charpy Impact, Notched  0.609 J/cm²
@Temperature -30.0 °C
2.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.609 J/cm²
@Temperature 22.8 °C
2.90 ft-lb/in²
@Temperature 73.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 86.6 kV/mm2200 kV/inIEC 60243-1
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.0 µin/in-°FISO 11359-2
Melting Point 170 °C338 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 110 °C176 - 230 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 3.50 - 7.03 MPa508 - 1020 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2128 / 310821

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.