MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Sintox ™ FA Metallizing Mac-A950R-3 Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Alumina ceramic with 95.0% Al2O3 content that is specially formulated for accurate grain size. This is feature particularly valuable when a ceramic microstructure is needed to provide a good keying surface for high integrity molybdenum metallizing.

Prime Features:

  • Dense, non-porous and vacuum tight
  • Readily accepts molybdenum metallizing for high temperature brazing of assemblies
  • High volume resistivity
  • Good high temperature characteristics
  • Low coefficient of expansion
  • Resists chemical attack
  • Fire resistant and non-outgassing
Typical Applications:
  • High vacuum equipment and scientific instruments where ceramic components need to be brazed to form high strength connections and complex assemblies
  • Insulators for probes and sensors
  • Transducer components
  • Insulators for vacuum pumps
  • Gun assemblies and connectors for X-ray tubes and electron microscopes
Production Capabilities:
  • Pressed and machined components
  • Metallizing of components
  • High temperature brazing of assemblies

Information provided by Morgan Advanced Materials

Key Words: Mac-A950R-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.75 g/ccfired
Open Porosity 0.00 %fully dense, % nominal, apparent
Grain Size >= 4.0 µmcontrolled limits; 8
 5.0 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell HR45N 78
Hardness, Vickers 12.5
@Load 0.500 kg
[GPa]
Modulus of Elasticity 325 GPa
Flexural Strength 320 MPa3-point; ASTM C1161
Compressive Strength 2000 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+8 ohm-cm
@Temperature 600 °C
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 9.4
@Frequency 9.40e+9 Hz
 9.5
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.50 µm/m-°C
@Temperature 0.000 - 800 °C
Thermal Conductivity 21.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 95 %
 
Descriptive Properties
Colorpink
Thermal Downshock170 sC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF5028 / 200266

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.