MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Braskem Unilene® B-100LN Low molecular weight, thermoplastic aromatic C9 hydrocarbon resin
Categories: Polymer; Thermoplastic

Material Notes: Low molecular weight, thermoplastic aromatic C9 hydrocarbon resin obtained through catalytic polymerization in a continuous process, pastillated in a pearl-like shape and presented in so yellow colored scale. Compatible with most solvents and polymeric materials. Unilene® B-100 LN has a controlled naphthalene content which allows for a less pronounced odor when compared to regular C9 hydrocarbon resins. In Rubbers, Unilene improves the processability of compounds, fillers incorporation, dispersion and tack of the mixture, avoiding the elastomer deterioration and reducing the preparation time. For applications in Hot Melt and Solvent-Based Adhesives, the resin promotes tack, wetting, cohesion, open time control and water repellency.
Applications: Hot melt adhesives (EVA, metallocene PE and PSA) and solvent based , In addition, the product can be used for seals and sealants, paints and varnishes (road marking, printing inks, aluminum and protective, epoxy and alkyd systems), rest and rubber artifacts and polymer modification.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10ASTM D974
 
Thermal PropertiesMetricEnglishComments
Softening Point 95.0 - 105 °C203 - 221 °FASTM D6493
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0ASTM D6166
 
Descriptive Properties
Naphthalene Content (ppm)100 maxInternal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS672 / 314065

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.