MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® AFA-6145 V0 Z PPA, 45% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: 45% glass fiber, flame retardant, high flow, hot-water molds

Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrared and vapor phase soldering operations typically used by the electronics industry.

Amodel® AFA-6145 V0 Z offers high flow and short molding cycles, thereby enhancing molding productivity and lowering costs.

- Black: AFA-6145 V0 Z BK 324
- Natural: AFA-6145 V0 Z NT

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Cell Phones; Connectors; Housings; Industrial Applications; Industrial Parts

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; Good Electrical Properties; Good Stiffness; High Flow; High Strength; Hot Water Moldability

Injection notes: Injection Rate: 3 to 4 in/sec
Adjust holding pressure to 1/2 injection pressure.
Set hold time to maximize part weight.
A general purpose screw is recommended, with minimum back pressure.
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³Method A; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 193 MPa28000 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Flexural Strength 276 MPa40000 psiASTM D790
Flexural Modulus 15.5 GPa2250 ksiASTM D790
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 1.59 mm
584 kV/in
@Thickness 0.0626 in
ASTM D149
Dissipation Factor 0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 400 - 599 V400 - 599 VPLC 1; UL 746
Hot Wire Ignition, HWI >= 120 sec>= 120 secPLC 0; UL 746
High Amp Arc Ignition, HAI 60 - 119 arcs60 - 119 arcsPLC 1; UL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 277 °C531 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.790 mm
V-0
@Thickness 0.0311 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 316 - 324 °C601 - 615 °F
Front Barrel Temperature 327 - 332 °C621 - 630 °F
Melt Temperature 321 - 338 °C610 - 640 °FInjection
Mold Temperature 66.0 - 93.0 °C151 - 199 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveFlame Retardant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
Injection RateFast
ProcessingWater-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4079 / 279879

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.