MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ineos T00G-02 Compounded Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: T00G-02 is a fraction melt flow TPO designed for the roofing membrane market. Its blend of impact resistance and flexural modulus is designed to provide an excellent balance between processing and performance. Typical applications include roofing membranes, geomembranes, mats, and applications that require flexibility and strength.
Availability: North America
Features: Food Contact Acceptable; Good Flexibility; Good Impact Resistance
Uses: Geo Membranes; Membranes
Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520
RoHS Compliance: Contact Manufacture
Forms: Pellets
Processing Method: Extrusion

Information provided by INEOS Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.877 g/ccASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 44ASTM D785
Tensile Strength at Break 1480 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 914 psi2.0 in/min; ASTM D638
Elongation at Break 810 %2.0 in/min; ASTM D638
Elongation at Yield 190 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 16400 psiASTM D790A
Izod Impact, Notched 6.50 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 11.0 ft-lb/in
@Temperature -20.0 °C
ASTM D256
Izod Impact, Notched (ISO) 16.1 ft-lb/in²
@Temperature 22.8 °C
Area; ASTM D256
 28.2 ft-lb/in²
@Temperature -20.0 °C
Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °FUnannealed; ASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINEOSA064 / 268300

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.