Key Features:- Extraordinary low temperature serviceability
- Room temperature cure
- Easy to handle
- Outstanding optical clarity
Product Description: MasterSil 415 is a one component acetoxy type, high performance silicone for bonding and sealing. It has a paste consistency and a non-drip application feature. MasterSil 415 is special in that it has excellent optical clarity along with superior non-yellowing properties. Also noteworthy is its low temperature serviceability; the range being from -185°F to +400°F. It bonds well to a wide variety of substrates such as glass, metals, many plastics, composites and various rubber materials including silicone. It is a faster curing system, although the speed is dependent on the thickness of the layer and the level of humidity. As a one part silicone, it has superb elasticity and flexibility. Also, it is a reliable electrical insulator. MasterSil 415 can be used in a wide variety of applications, particularly when silicone type flexibility along with low temperature serviceability and/or transparency are desirable.Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |