MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool® Pyro-Fold ™ and Pyro-Stack™ 607 HT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool Pyro-Fold and Pyro-Stack modules are made from Superwool blankets. These modules come with the same internal hardware as offered in the Superwool Pyro-Bloc Y and M modules. Superwool Pyro-Fold and Pyro-Stack modules offer an alternative to traditional solutions due to its high refractoriness and provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Applications:

  • Homogenizing furnaces
  • Process heaters
  • Ceramic kiln
  • Annealing furnace
  • Heat treating furnace
  • Thermal oxidizers

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.128 g/cc
 0.149 g/cc
 0.172 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0300 W/m-K
@Temperature 816 °C
ASTM C201
 0.0700 W/m-K
@Temperature 260 °C
ASTM C201
 0.150 W/m-K
@Temperature 538 °C
ASTM C201
Maximum Service Temperature, Air 1150 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
CaO 18 - 25 %
Other <= 3.0 %
SiO2 70 - 80 %
 
Descriptive Properties
Classification Temperature (°C)1300
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF70108 / 203406

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.