MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Angst+Pfister APSOplast® PVC-U Transparent Plastics
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Transparent

Material Notes:

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DIN EN ISO 1183-1
Moisture Absorption 0.200 %0.200 %50 % r.h.; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282DIN EN ISO 868
Ball Indentation Hardness 120 MPa17400 psiDIN EN ISO 2039-1
Tensile Strength 30.0 MPa4350 psi50 mm/min; DIN EN ISO 527
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 10 %>= 10 %50 mm/min; DIN EN ISO 527
Elongation at Yield 3.0 %3.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 3.00 GPa435 ksi1 mm/min; DIN EN ISO 527
Flexural Strength 90.0 MPa13100 psi2 mm/min; ISO 178
Charpy Impact Unnotched NBNBDIN EN ISO 179-1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.03.0IEC 60250
Dielectric Strength 20.0 - 40.0 kV/mm508 - 1020 kV/inIEC 60243
Dielectric Loss Index 0.0100.010IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN 53752
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 60.0 °C140 °F
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FDIN EN ISO 75
Minimum Service Temperature, Air -15.0 °C5.00 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 88 %
@Thickness 3.00 mm
88 %
@Thickness 0.118 in
DIN 5036 / ASTM D-1003 / ISO 13468-1/-2
 
Descriptive Properties
Colorclear transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP014 / 250512

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.