System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Celanex® 4202 PBT, 15% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Material Notes:
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.38
g/cc
ASTM D792
Density
1.38
g/cc
ISO 1183
Moisture Absorption
0.160 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.0040
cm/cm
ISO 294-4
0.0050
-
0.010
cm/cm
ASTM D955
Linear Mold Shrinkage, Transverse
0.0090
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
86.0
MPa
5mm/min; ISO 527-2/1A
12200
psi
ASTM D638
Tensile Strength, Yield
12400
psi
ASTM D638
Elongation at Break
3.8 %
ASTM D638
4.4 %
5mm/min; ISO 527-2/1A
Tensile Modulus
5200
MPa
50mm/min; ISO 527-2/1A
700000
psi
ASTM D638
Flexural Strength
141
MPa
ISO 178
20400
psi
ASTM D790
Flexural Modulus
5100
MPa
ISO 178
640000
psi
ASTM D790
Izod Impact, Notched
1.80
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
11.7
kJ/m²
ISO 180/1A
Charpy Impact Unnotched
52.0
kJ/m²
ISO 179/1eU
37.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
10.7
kJ/m²
ISO 179/1eA
5.70
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
2.00e+16
ohm-cm
IEC 60093
Surface Resistance
1.00e+17
ohm
IEC 60093
Dielectric Constant
3.2
@Frequency 1e+6 Hz
IEC 60250
3.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength
22.0
kV/mm
IEC 60243-1
Dissipation Factor
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
>=
600
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
36.0
µm/m-°C
ISO 11359-2
CTE, linear, Transverse to Flow
100
µm/m-°C
ISO 11359-2
Melting Point
225
°C
10°C/min; ISO 11357-1,-2,-3
437
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
216
°C
ISO 75-1, -2
420
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
183
°C
ISO 75-1, -2
380
°F
ASTM D648
Glass Transition Temp, Tg
44.0
°C
ISO 11357-1,-2,-3
Flammability, UL94
HB
Processing Properties
Original Value
Comments
Processing Temperature
65.0
-
93.0
°C
cavity
250
-
260
°C
hot runner
Feed Temperature
230
-
240
°C
Zone 1
230
-
240
°C
Zone 2
235
-
250
°C
Zone 3
235
-
250
°C
Zone 4
240
-
260
°C
Die Temperature
250
-
260
°C
Melt Temperature
235
-
260
°C
260
°C
ISO 294
Mold Temperature
82.0
°C
ISO 294
Injection Velocity
300
mm/sec
ISO 294
Drying Temperature
120
-
130
°C
Dry Time
4.00
hour
Moisture Content
<= 0.020 %
Hold Pressure
48.0
MPa
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber
Hippe PA 46 Nylon 46
RTP Company RTP 1003 FR A Polybutylene Terephthalate (PBT), Glass Fiber - Flame Retardant - UL94 V-0
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced
Kingfa PBT-RG20 Flame Retardant, 20% Glass Fiber Reinforced PBT
PHCQ065 / 178520
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.