MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyolefin

Material Notes:

Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 0.892 g/cc0.892 g/ccASTM 792
    Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
    Melt Flow 2.75 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    2.75 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 515110 seconds; ASTM D2240
    Tensile Strength, Ultimate 13.4 MPa1950 psiASTM D638
    Elongation at Break 650 %650 %ASTM D412
    Flexural Modulus, 1% Secant 414 MPa60000 psiASTM D790
    Tear Strength 99.9 kN/m570 pliASTM D624
     
    Thermal PropertiesMetricEnglishComments
    Brittleness Temperature -50.0 °C-58.0 °FASTM D746
    Flame Spread 13.4 mm/min0.528 in/minFM VSS-302
     
    Descriptive Properties
    FoggingMin. 90SAE-J275

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    RTP Company Permaprene™ 2800 B-85A Thermoplastic Polyolefin Elastomer (TEO)
    Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
    Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer

    PMULTI095 / 53999

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.