MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon L4930TC HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Alathon L4930TC is a bimodal high density polyethylene copolymer natural resin used by customers for telecommunications conduits. L4930TC offers an excellent balance of stiffness, toughness and ease of processing. Conduits made with this resin are used with fiber optic cable, electrical cable and telecommunications cable. L4930TC meets the material requirements for polyethylene conduit as per ASTM F2160 and also meets the requirements of ASTM D3350 cell classification 435540A.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
ESCR 100% Igepal® >= 600 hour>= 600 hourCond C, F20; ASTM D1693
 >= 1000 hour>= 1000 hourCond B, F50; ASTM D1693
ESCR 10% Igepal® >= 1000 hour>= 1000 hourCond B, F50; ASTM D1693
Melt Flow  0.300 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.300 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 1.10 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.10 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 26.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
26.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63.063.0ASTM D2240
Tensile Strength, Yield 24.8 MPa3600 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus 0.938 GPa136 ksi2% Secant; ASTM D790
Tensile Impact 148 J/cm277 ft-lb/inASTM D1822
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9037 / 323965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.