MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.

Applications: For use in applications which require exposure to temperatures in excess of 260°C (500°F) and shorter term to 310°C (590°F). Recommended for use in the semiconductor industry. Do not use any Perlast ® grade with molten alkali metals.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63°IRHD, -7 change after 72 hours @ 260°C; ASTM D1415
 70°IRHD; ASTM D1415
Tensile Strength, Yield 14.7 MPaASTM D412
 17.346 MPa18% change after 72 hours @ 250°C; ASTM D412
Elongation at Break 192 %-4% change after 72 hours @ 250°C; ASTM D412
 200 %ASTM D412
100% Modulus 0.008184 GPa
@Strain 100 %
-12% change after 72 hours @ 250°C; ASTM D412
 0.00930 GPa
@Strain 100 %
ASTM D412
Compression Set 17 %
@Temperature 200 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 310 °C
Minimum Service Temperature, Air -15.0 °C
Flash Point >= 400 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer

PPRECI008 / 57732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.