MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, > 50 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: AMPCOLOY 940 is a patented alloy which meets the demands of users of the RWMA class 3 alloys without Beryllium. In the industrialized countries, stricter health and safety instructions on the use of noxious elements have forced AMPCO to develop this new alloy. It replaces the AMPCOLOY 95 in practically all applications.

Applications: AMPCOLOY 940 is used wherever a good electrical or thermal conductivity is required together with high mechanical properties: Electrode holders and seam welding shafts; Spot welding electrodes, seam welding discs, projection and butt welding dies, principally for stainless steel and Monel; Plunger tips for cold chamber aluminum die casting machines; Parts of moulds for injection moulding of plastics, injection-nozzles and cooling pins; Brake drums for paper winding rolls; Parts for energy engineering

Key Words: RWMA Class 3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.71 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 210HB 30
Hardness, Rockwell B 95
Tensile Strength, Ultimate 662 MPa
Tensile Strength, Yield 510 MPa
@Strain 0.5 %
Elongation at Break 13 %
Reduction of Area 20 %
Modulus of Elasticity 131 GPa
Compressive Yield Strength 552 MPa0.1% Perm. Set
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000357 ohm-cm48% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.5 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 208 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr <= 0.40 %
Copper, Cu 96.4 - 96.8 %As Balance
Nickel, Ni 2.5 %
Silicon, Si 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, ≤ 25 mm.
Performance Alloys MoldStar® 90 Copper Mold Alloy
Ampco Metal AMPCO® M4 Nickel-Aluminum Bronze, Extrusion, 25.4 - 101.6 mm.
Ampco Metal AMPCOLOY® 944 MoldMATE Nickel-Copper

NAMPCO42 / 14996

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.