MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
Categories: Metal; Metal Matrix Composite

Material Notes: AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements include high strength, lightweight, custom CTE and high thermal conductivity. PCC offers AlSiC with a composition varying between 30% to 74% silicon carbide by volume, depending on the application. This flexible material system allows PCC Composites to produce a part that can be tailored to exact solution requirements.

Infomation provided by PCC-Advanced Forming Technology.

Key Words: Aluminum/Silicon Carbide MMC; Al/SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.04 g/cc0.110 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9999
Tensile Strength, Ultimate 205 MPa29700 psi
Modulus of Elasticity 230 GPa33400 ksi
Fracture Toughness 10.6 MPa-m½9.65 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C
@Temperature 20.0 - 30.0 °C
3.89 µin/in-°F
@Temperature 68.0 - 86.0 °F
Thermal Conductivity 175 W/m-K1210 BTU-in/hr-ft²-°F
Melting Point 557 - 613 °C1030 - 1140 °F
Solidus 557 °C1030 °F
Liquidus 613 °C1140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PCC-Advanced Forming Technology 30% AlSiC Metal Matrix Composite
Ceramic Process Systems AlSiC-9, 63 vol% SiC
Ceramic Process Systems AlSiC-8, 70 vol% SiC
PCC-Advanced Forming Technology 63% AlSiC Metal Matrix Composite
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite

NZMPC2 / 20042

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.