MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchkote™ 60EG 533 Urethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Scotchkote Urethane Elastomer 60EG 533 has been specifically developed as an elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.

Product Features:

  • Physical properties similar to factory produced rubbers
  • Deigned for application by trowel or spatula at thicknesses up to 6 mm
  • Good cold vulcanizing capabilities
  • Suitable for use to repair conveyor belts, rollers, gaskets, hoses, etc.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Thickness 6100 microns240 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength at Break 6.89 MPa999 psi
Elongation at Break 800 %800 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.0 kV/mm406 kV/in
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourInitial Set
 960 min16.0 hourMachining Time
 4320 min72.0 hourFull Mechanical
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast
Northstar Polymers MPC-W44A Polyurethane Gel
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Freudenberg Hydrolysis-Resistant Polyurethane Elastomer

PMM35302 / 170049

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.