MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Astralloy EB-450® Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: EB-450® is a liquid quenched and tempered, through-hardened up to 3”, high impact alloy steel with excellent abrasion-resistant properties. Its balanced boron, modified nickel-chrome moly chemistry is ideal for achieving an optimum hardness to toughness ratio. EB-450 boasts a longer wear life due to its through-hardness which is more uniform than what is found in conventional carbon/ manganese steels. This quench-hardened material is competitively priced for optimum cost/wear rations. The resistance to atmospheric corrosion further reduces surface pitting. EB-450 is field proven in extremely abrasive bulk handling installations.

Benefits:

  • Higher wear resistance, when compared to conventional steels, due to its uniform hardness.
  • Easy to weld with normal low hydrogen simple techniques.
  • May be flame cut with oxyacetylene, plasma or similar methods.
  • Cold formable with heavy presses or rolls.
  • The high hardness and toughness in combination with its low friction coefficient, reduces maintenance costs.
  • EB-450 may be easily cut, welded, machined and cold formed, as required.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 418 - 495
Tensile Strength 235 ksi
Tensile Strength, Yield 190 ksi
Elongation at Break 12 %
@Thickness 50.8 mm
Reduction of Area 42 %
Charpy Impact 20.0 ft-lb
@Temperature -40.0 °C
 28.0 ft-lb
@Temperature 23.9 °C
Bend Radius, Minimum 6.0 tPerpendicular to Rolling Direction
 12 tParallel to Rolling Direction
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.27 %
Chromium, Cr <= 1.75 %
Iron, Fe >= 95.7 %As Balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.30 %
Nickel, Ni <= 0.70 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.20 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astralloy 4800® Wear Resistant Steel
Astralloy 4330 V-Mod Alloy Steel Round Bars
Astralloy 8000® Abrasion-Resistant Steel
Astralloy 4145 H-Mod Alloy Steel Round Bars
AISI 4340 Steel, oil quenched 800°C (1470°F), 650°C (1200°F) temper, 50 mm (2 in.) round

NNUCOR903 / 233177

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.