MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oceanchem Group Melamine Cyanurate (MCA)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C6H9N9O3

Cas No.: 37640-57-6

Physical Appearance: Fine, white, crystalline powder, nontoxic, odorless; indissolvable in water and most organic solvents.

Use: Melamine Cyanurate is a halogen-free flame retardant for polyamide. Melamine Cyanurate has established itself as the flame retardant to achieve UL 94 V-0 especially for polyamide 6 and 6,6. Addition of MCA gives PA6(66) good mechanical and electrical properties. Being halogen free also results in significant advantages in terms of fire safety, i.e. lower smoke density, lower smoke toxicity and less corrosion.

Features: Steady color, good electrical properties, environmentally friendly.

Storage and Transportation: Handle with care, keep airtight and dry.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/cc
Bulk Density 0.300 - 0.400 g/cc
Brightness 96.0 %Whiteness
pH 5.0 - 7.0
Molecular Weight 255.2 g/mol
 
Descriptive Properties
CAS Number37640-57-6
MCA (%)99.5
Molecular FormulaC6H9N9O3
Residue (%)0.001Melamine
 0.2Cyanuric acid
Solubility0.002g/100ml water, at 20°C
Weight Loss (%)0.2dry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Perstorp Compounds Aminel FX Melamine
Chengdu Polyster MCA Melamine Cyanurate
Raschig Group MELOPLAS® 182 MF
Raschig Group MELOPLAS® 181.5 MF
Raschig Group MELOPLAS® 181 MF

POCEAN19 / 104223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.