MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CHR® M-Series (1 Mil PET/Rubber adhesive) is manufactured from polyester film with rubber pressure-sensitive adhesive.

Features/Benefits: M897 features a highly cross-linked pressure sensitive silicone adhesive system that eliminates adhesive legging and transfer in application and high-tack adhesive system offers masking protection. The thermosetting rubber adhesive system offers excellent quick-stick properties and flag resistance, yet unwinds easily. The polyester backing resists damage from sharp edges. Polyester backings offer low-cost, effective holding for materials. Operating temperature is -18 to +163 °C, elongation % at break is 100, tensile strength is 44N/cm and dielectric strength is 5,000 volts. M897 has an operating temperature of -18 to +177 °C, and ESD controlled static charge of <50 volts for removal from roll and board.

Applications: M897 offers economical methods to hold, insulate and/or protect various materials.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 100 %100 %
Tear Strength 4.38 kN/m25.0 pliInitial Tear Strength
Peel Strength 0.220 kN/m1.26 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 5000 V5000 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 163 °C325 °F
Minimum Service Temperature, Air -17.8 °C0.000 °F
 
Descriptive Properties
ColorOlive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® SG56-05(R) Anti-Static Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® SG25-05(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® K250 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2916-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape

PSTGQZ327 / 68841

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.