MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Star Plastics PCGF30 Molding Grade PC with 30% Glass
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Information provided by Star Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17000 psiASTM D638
Tensile Modulus 900000 psiASTM D638
Flexural Yield Strength 21500 psiASTM D790
Flexural Modulus 925000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/in73°F, 0.125 in.; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 290 °Funannealed, .125in; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 550 - 600 °F
Middle Barrel Temperature 575 - 625 °F
Front Barrel Temperature 600 - 650 °F
Nozzle Temperature 600 - 650 °F
Melt Temperature 600 - 650 °F
Mold Temperature 175 - 225 °F
Drying Temperature 250 °F
Dry Time 4 hour
Back Pressure 50.0 - 200 psi
Screw Speed 40 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Star Plastics PCGF20 Molding Grade PC with 20% Glass
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass

PSTARP21 / 68585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.