MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ Ultra LD 705.MJ molding Ethylene Vinyl Acetate Copolymer (EVA)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Escorene Ultra LD 705.MJ molding is a fractional melt index, 12.8 wt % vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles, and compounds. 

Availability:  Asia Pacific, Latin America, North America. 

Additive:  thermal stabilizer: yes. 

Applications:  bonding adhesives, flexible hoses, tube extrusion, compounding, profile extrusion, viscosity modifier.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccASTM D1505
Vinyl Acetate Content 12.8 %ExxonMobil Method
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 36
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 2300 psiASTM D638
Tensile Strength, Yield 1000 psiASTM D638
Elongation at Break 660 %ASTM D638
Elongation at Yield 110 %ASTM D638
Flexural Modulus, 1% Secant 12000 psiASTM D790
Dart Drop, Total Energy 15.0 ft-lb
@Temperature 22.8 °C
Instrumented; ASTM D3763
 17.0 ft-lb
@Temperature -40.0 °C
Instrumented; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 201 °FPeak; ExxonMobil Method
Vicat Softening Point 167 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98908 / 238290

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.