MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Potassium Chloride (KCl)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.98 g/cc
a Lattice Constant 6.292 Å
c Lattice Constant 6.292 Å
Molecular Weight 74.55 g/mol
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 150MPa
Hardness, Mohs 2.0
Modulus of Elasticity 16.8 GPain <110> direction
 38.2 GPain <100> direction
Poissons Ratio 0.134
Shear Modulus 6.30 GPain <110> direction
 10.8 GPain <100> direction
 
Thermal PropertiesOriginal ValueComments
CTE, linear 34.1 - 38.3 µm/m-°C
@Temperature -60.0 - 60.0 °C
Specific Heat Capacity 0.695 J/g-°C
Thermal Conductivity 6.53 W/m-K
@Temperature 46.0 °C
Melting Point 776 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4546at n10.6
 1.2626
@Wavelength 30000 nm
 1.4325
@Wavelength 15000 nm
 1.4796
@Wavelength 1000 nm
 1.493
@Wavelength 546.1 nm
at ne
 1.717
@Wavelength 200 nm
IR Transmittance 68 %
@Wavelength 20000 nm
Internal Transmittance
 98 %
@Wavelength 1000 nm
Internal Transmittance
 98 %
@Wavelength 12000 nm
Internal Transmittance
UV Transmittance 89 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(100)perfect
Constants of Elastic Compliance (Pa^-1)1.6198E-10S44
 2.621E-11S11
 -3.47E-12S12
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-3.28E-5 to -3.75E-5at 3.39 microns for ± 60°C
Transmission Range (microns)0.21 - 21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potassium Chloride, KCl (Sylvite)
Sodium Chloride, NaCl (Halite)
Magnesium Chloride, MgCl2 (Chloromagnesite)
Mateck Sodium Chloride (NaCl)
Lead (II) Sulfide, PbS

CMAT050 / 87734

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.