MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation RO3730 Antenna Grade Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of 0.0013 measured at 2.5 GHz. These values allow antenna designers to realize substantial gain values while minimizing signal loss. Materials are available with a demonstrated low PIM performance, with values better than -154 dBc (measured using Rogers' internal test method).

Cladding is 1 ounce rolled annealed copper (35 microns thick).

Features and Benefits:

  • RO3730 reinforced woven fiber glass with optimized glass and filler loading - Improved mechanical rigidity, easier handling and processing versus non-reinforced PTFE products and lower dissipation factor
  • Low PIM - reduced signal interference
  • Loss - improved antenna gain
  • Economically priced - volume manufacturing
  • Environmentally friendly - Lead-free process compatible and RoHS compliant

Typical Applications:

  • Base station antennas
  • RFID antennas
  • WLAN antennas
  • Satellite Radio antennas

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.10 g/ccASTM D792
Moisture Absorption at Equilibrium 0.040 %D48/50; ASTM D570
Thickness 30.0 - 60.0 milRange of Thicknesses Available
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 8.00 MPaY-Direction; IPC-TM-650, 2.4.4
 9.00 MPaX-Direction; IPC-TM-650, 2.4.4
Peel Strength 10.5 pli
@Temperature 288 °C,
Time 10.0 sec
Copper, After Solder Float; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmCond. A; IPC 2.5.17.1
Surface Resistance 1.00e+13 ohmCond. A; IPC 2.5.17.1
Dielectric Constant 2.93
@Frequency 8.00e+9 - 4.00e+10 Hz
Z direction, Design; Differential Phase Length Method
 2.94 - 3.06
@Frequency 1e+10 Hz
Z direction, Process; IPC-TM-650 2.5.5.5
Dissipation Factor 0.0013
@Frequency 2.50e+9 Hz
IPC-TM-650 2.5.5.5
 0.0016
@Frequency 1e+10 Hz
IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°CX-Direction; IPC-TM-650 2.4.41
 12.0 µm/m-°CY-Direction; IPC-TM-650 2.4.41
 65.0 µm/m-°CZ-Direction; IPC-TM-650 2.4.41
Thermal Conductivity 0.450 W/m-KD24/23; IPC-TM-650, 2.6.2.1
Decomposition Temperature 500 °CASTM D3850
Flammability, UL94 V-0
 
Descriptive Properties
Dimensional Stability0.02 mm/mX direction; IPC-TM-650, 2.4.39A
 0.03 mm/mY direction; IPC-TM-650, 2.4.39A
PIM< -154 dBc
Thermal Coefficient of Dielectric Constant-22 ppm/°C-50°C to 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled

PROGA953 / 138393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.