MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei TENAC™-C TFC77 Copolymer Acetal (POM), Electrically Conductive
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Excellent balance of mechanical properties, low friction and wear characteristics. Applications: Automotive parts, electrical & electronic parts, industrial parts.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm0.012 - 0.016 in/inAsahi Kasei
Melt Flow 1.0 g/10 min1.0 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 38.0 MPa5510 psi50% RH; ISO 527
Elongation at Break 3.0 %3.0 %50% RH; ISO 527
Tensile Modulus 3.20 GPa464 ksi50% RH; ISO 527
Flexural Modulus 3.10 GPa450 ksi50% RH; ISO 178
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.0 - 10 ohm-cm1.0 - 10 ohm-cmIEC 60093
Surface Resistance 1.0 - 10 ohm1.0 - 10 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei TENAC™-C C84 Copolymer Acetal (POM), Electrically Conductive
Abatron AboCoat 8709-7 Nickel-Filled Electrically Conductive Acrylic Compound
Asahi Kasei TENAC™-C TFC64 Copolymer Acetal (POM), Electrically Conductive
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic

PASAHI8118 / 221145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.