MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products BC 9060 Silicone RTV Rubber
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high tear with good elongation. Application: BC 9060 is a mold-making material recommended for repetitive production of intricate shapes cast in epoxy or urethane resins. It is also used in the potting of electronic components and in protecting sensitive assemblies against thermal shock and vibration. Deaeration: Air entrapped during the mixing cycle must be removed to eliminate voids in the cured compound. Place the mixture in a vacuum of 29 inches of mercury. The mixture will expand to 4-5 times its original volume, crest and recede approximately to its original level. Continue the deaeration for an additional 1-2 minutes and the material will be ready to use. Cured Compatibility: cure inhibition (poisoning) of BC 9060 may be caused by various materials used in the master pattern. When the BC 9060 comes in contact with such materials as sulphur containing clays, phosphorous, nitrogen containing materials, organometallic salt (Dibutyl-tin dilaurate, etc.) certain organic adhesives and tapes, cure is hindered. This condition is characterized by a gummy appearance in the surface of the silicone rubber at the interface of the silicone and substrate. A pretest of compatibility is recommended for each suspect substrate to determine whether a barrier coat or other inhibition prevention measure is necessary.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/cc
Brookfield Viscosity 10000 cPMixed
 140000 cP
@Temperature 25.0 °C
Compound
Linear Mold Shrinkage 0.0010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength, Ultimate 800 psi
Elongation at Break 200 %
Tear Strength 90.0 pli
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -75.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 60.0 °C
10% cure
 24.0 min
@Temperature 60.0 °C
90% cure
Pot Life 120 min
@Temperature 25.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Mix Ratio10:1 by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Humiseal 1C49 Silicone Conformal Coating

PBCC060 / 107287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.