System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
;
Linear Low Density Polyethylene (LLDPE), Injection Molded
Material Notes:
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.
Applications:
Thin walled container lids and closures.
Data provided by the manufacturer.
Key Words:
Linear Low Density Polyethylene
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.931
g/cc
ASTM D792
Melt Flow
105
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow
45.7
cm
NOVA Snake Flow Test
Mechanical Properties
Original Value
Comments
Hardness, Shore D
56
ASTM D2240
Tensile Strength, Yield
14.0
MPa
ASTM D638
Flexural Modulus
0.520
GPa
ASTM D790
Thermal Properties
Original Value
Comments
Vicat Softening Point
100
°C
ASTM D1525
Brittleness Temperature
-30.0
°C
ASTM D746
Processing Properties
Original Value
Comments
Melt Temperature
170
-
260
°C
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 3272 Polyethylene, Injection Grade
Huntsman PE2080 Injection Molding Polyethylene
Huntsman PE2075 Injection Molding Polyethylene
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Dow HDPE 65053N High Density Polyethylene
PEHN1J / 35568
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.