MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KLJ Group KLJ HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description: KLJ-HDPE UV Black is a High-Density Polyethylene (HDPE) compound developed to be used for sheathing of Fiber Optic Cables (OFC) / PIJF & Power cables. It has been formulated with necessary additives and processing aid to achieve good extrusion. The incorporation of 2.5% of Carbon black gives the UV and light stabilization required for the compound and the cables it is used on.

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.945 - 0.952 g/ccASTM D792
Melt Flow <= 1.0 g/10 min
@Load 2.16 kg
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 15.0 MPaIS 10810 Part-7
Elongation at Break >= 767 %IS 10810 Part-7
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 2.00e+16 ohm-cmIS 3396
Dielectric Constant <= 2.1IEC 60250
Dielectric Strength 36.6 kV/mmIEC 60243
Dissipation Factor <= 0.00090IEC 60250
 
Thermal PropertiesOriginal ValueComments
Shrinkage <= 0.50 %
@Temperature 77.0 - 83.0 °C,
Time 18000 sec
IS 7098
 
Descriptive Properties
Content57 ppmASTM E203

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ337 / 284358

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.