MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Durostone®-Glastic MTS Polyester, E-glass roving fibers
Categories: Polymer; Thermoset; Polyester, TS

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 - 2.00 g/ccASTM D792
Filler Content 50 - 60 %glass
Water Absorption 0.30 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 344.5 MPaParallel; ASTM D5083
Modulus of Elasticity 22.0 - 26.0 GPaPerpendicular; ASTM D790
Tensile Modulus 13780 psiParallel; ASTM D5083
Flexural Strength 400 - 500 MPaPerpendicular; ASTM D790
Compressive Strength 96.5 MPaPerpendicular; ASTM D695
 200 - 300 MPaParallel; ASTM D695
Shear Strength 2000 psiin plane; ASTM D3846/D3914
Izod Impact, Notched 40.0 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 5.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 2.80 kV/mm
@Thickness 25.4 mm
axial in oil; ASTM D149
Arc Resistance 130 secASTM D495
Comparative Tracking Index 500 VASTM D3628/UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°CASTM D696
Thermal Conductivity 0.290 W/m-KASTM C177
Maximum Service Temperature, Air 311 °F
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9101 / 232804

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.