MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Laborplast UPVC-INJ COMPOUND for injection molding Recycled Polyvinyl Chloride
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: UPVC-INJ compound is used to produce injection-molded items and designed to obtain a product with excellent aesthetic features without impacting ease of processing or mechanical performance. UPVC-INJ formulations are predominantly made from milled post-industrial window profiles, calendered, thermoformed and injection-molded items. During the process, additives such as paraffin waxes, Ca/Zn stabilisers and shock-absorbing agents are used to improve the product’s processability and technical performance. This compound’s main applications are technical items and construction fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Tolerance: ±0.8; ISO 1183-1
Melt Flow 30 g/10 min30 g/10 minTolerance: ±5; ISO 1133/G
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.0 MPa3630 psiTolerance: ±5; ISO 527-1
Tensile Strength, Yield 40.0 MPa5800 psiTolerance: ±5; ISO 527-1
Elongation at Break 100 %100 %Tolerance: ±30; ISO 527-1
Tensile Modulus 2.20 GPa319 ksiTolerance: ±0.2; ISO 527-1
Flexural Strength 55.0 MPa7980 psiTolerance: ±3; ISO 178
Flexural Modulus 2.00 GPa290 ksiTolerance: ±0.2; ISO 178
Impact 1111[kJ/m2], Tolerance: ±0.5; ISO 180/5.55
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 5.0 MPa 53.0 °C127 °FTolerance: ±4; ISO 75/C
Vicat Softening Point 73.0 °C163 °FTolerance: ±4; ISO 306/B
 
Descriptive Properties
Thermal stability60 minTolerance: ± 10; ISO 182-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLABO02 / 318002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.