MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TBA ECP 12E Stainless Steel Fiber Masterbatch EMI Shielding Thermoplastic
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: ECP 12E is a stainless steel fiber masterbatch within an emulsion-based ethylene acrylic acid zinc ionomer binder, 25% by weight. It can be used with Styrenic Thermoplastics, PS,SAN, ABS also PPO and PPE Alloys, Polypropylene/Polyolefines. Other binders are available - ECP 16E using nylon 6/12 binder 25% by weight for use with nylon 6, 6/6, 6/10 6/12, PBT, PET. ECP 20E with a polycarbonate binder 40% by weight, for use with polycarbonate, polysulphone, PES, PET, PEJ, PBT. The masterbatch is added at very low levels ensuring minimal effect on color, moldability and other base polymer properties by 1% by volume. The use of this system allows EMI shielded articles to be produced in one process without additional equipment, labor or secondary processing and provides cost effective solution to EMI shielding problems.

Features:

  • No secondary process
  • Used in any plastic molding application
  • Can be colored (but not suitable for bright colors such as yellow, white etc)
  • Provides shielding of 50dB attenuation
Benefits:
  • Cost effective
  • Non-abrasive
  • Minimal effect on color
  • Eliminates secondary EMI shielding process
Material Specification:
  • A masterbatch pellet
  • Stainless steel fiber AIS1304, bonded with polymer specific binder
  • In pellet form, 5mm chopped length

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 32.3 MPa4680 psi
Elongation at Break 3.5 %3.5 %
Tensile Modulus 2.36 GPa342 ksi
Flexural Strength 58.0 MPa8410 psi
Flexural Modulus 2.19 GPa318 ksi
Izod Impact, Notched 0.551 J/cm1.03 ft-lb/in
Charpy Impact Unnotched 1.59 J/cm²7.57 ft-lb/in²
Charpy Impact, Notched 0.710 J/cm²3.38 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTBA016 / 281494

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.