MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Cusil™ Mac-Cusil™-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: High-purity silver/copper alloy for vacuum brazing.

Applications: High-integrity brazed joint duties in:

  • Aero-engines (OEM and repair)
  • Aerospace fuel-line assemblies
  • Vacuum tubes
  • Wave guide and Klystron assemblies
  • Power supply surge arrestors
  • Automotive components
`

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.361 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 1010expressed as Mpa
Tensile Strength 372 MPa
Elongation at Break 19 %2 in/50mm gage section
Modulus of Elasticity 83.0 GPa
Compressive Yield Strength 272 MPa0.2% offset
Poissons Ratio 0.36calculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000204 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.6 µm/m-°C
@Temperature 20.0 - 500 °C
Thermal Conductivity 371 W/m-Kcalculated
Melting Point 780 °C
Solidus 780 °C
Liquidus 780 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 28 %nominal
Silver, Ag 72 %nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Mac-Copper OFHC-WM Braze Alloy
Morgan Advanced Ceramics Incusil™ Mac-Incusil™ ABA-WM Braze Alloy
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics 50Au-50Cu Mac-560Au/50 Cu-WM Braze Alloy

CMORF8012 / 203489

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.