MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucite International Elvacite® 2042 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2042 is a very high molecular weight ethyl methacrylate polymer. It is a tough, alcohol – tolerant, broadly compatible grade for use in abrasion – resistant coatings such as high – gloss clear lacquers for decals and outdoor signs. Slightly softer than Elvacite® 2013.

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
Particle Size 110 - 180 µm
Molecular Weight 220000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.00
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 37.2 MPa
Elongation at Break 25 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 65.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Elvacite® 2045 Acrylic Resin
Lucite International Elvacite® 2044 Acrylic Resin
Lucite International Elvacite® 2043 Acrylic Resin
Lucite International Elvacite® 2016 Acrylic Resin

PLUCIT9459 / 150173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.